epoxy-floor-coating-comparison--colored-sand-self-leveling-8-colours-ce/isoepoxy-colored-sand-self-leveling-floor-coating--standard-grade-25kg-8-colours, epoxy-floor-coating-comparison--colored-sand-self-leveling-8-colours-ce/isoepoxy-colored-sand-self-leveling-floor-coating--standard-grade-25kg-8-colours, /epoxy-colored-sand-floor-coating
Inquiry
epoxy-floor-coating-comparison--colored-sand-self-leveling-8-colours-ce/isoepoxy-colored-sand-self-leveling-floor-coating--standard-grade-25kg-8-colours, epoxy-floor-coating-comparison--colored-sand-self-leveling-8-colours-ce/isoepoxy-colored-sand-self-leveling-floor-coating--standard-grade-25kg-8-colours, 
Inquiry

Epoxy Colored Sand Self-Leveling Floor Coating – Standard Grade, 25kg, 8 Colours

Standard grade epoxy colored sand self-leveling floor coating, 25kg bucket. Granite-effect speckled finish in 8 standard colours (HC51-011 to 018). Chemical resistant, wear resistant, seamless floor for factories, warehouses, and car parks. MOQ 1 ton. CE certified.

Request a Quote
  • Overview

Overview

Epoxy Floor Coating Comparison: Selecting the Right System for Industrial Use

An accurate epoxy floor coating comparison evaluates compressive strength, chemical resistance, dry film thickness, installation requirements, certification status, and total lifecycle cost — not unit price alone. This structured overview positions the Epoxy Colored Sand Self-Leveling Floor Coating (Standard Grade) against standard alternatives across the dimensions that determine long-term performance in warehouse, factory, and logistics environments.

Product Overview

A two-component epoxy system blended with coloured quartz sand aggregate. The system layers an epoxy primer, a base coat with broadcast quartz sand, and a self-leveling topcoat that flows to a smooth, uniform finish with minimal trowelling. This self-leveling characteristic reduces installation skill requirements and produces consistent surface quality across large floor areas without specialist equipment — a practical advantage for high-volume industrial floor projects.

epoxy-colored-sand-floor-coating-1.png

Epoxy Floor Coating Comparison: Performance Dimensions

vs. Standard Epoxy Paint — Strength and Lifecycle Cost

Standard single-coat epoxy floor paint delivers 0.1–0.3 mm dry film thickness, suited to light-duty environments. This self-leveling system delivers 1.5–3.0 mm DFT and ≥ 70 MPa compressive strength — a measurable performance gap under sustained industrial traffic. From a warehouse floor ROI perspective, standard paint in heavy-use environments typically requires recoating every two to three years; the self-leveling system's extended service life generally recovers its cost premium over a five-to-seven year evaluation period through reduced recoating frequency and lower facility downtime.

Chemical Resistant Quartz Sand Coating vs. Thin-Film Systems

Where floors face routine exposure to oils, fuels, dilute acids, or alkalis, the chemical resistant quartz sand coating provides protection that thin-film alternatives are not designed to deliver. The cured two-component epoxy matrix with embedded quartz aggregate resists chemical penetration while maintaining surface integrity under heavy traffic. Formulation chemistry matters as much as film thickness — this system is engineered specifically for industrial chemical exposure environments.

Technical Specifications

Parameter Value
Type Two-component epoxy + coloured quartz sand
Finish Granite speckle self-leveling
Standard Colours 8 colours (HC51-011 to HC51-018)
Dry Film Thickness 1.5–3.0 mm
Compressive Strength ≥ 70 MPa
Tensile Bond Strength ≥ 1.5 MPa
Abrasion Resistance ≤ 0.03 g (Taber CS-17, 1000 cycles)
Chemical Resistance Oils, fuels, dilute acids & alkalis
Application Rate 3.0–5.0 kg/m²
Packaging 25 kg/bucket
MOQ 1 ton
Certifications CE, ISO 14001

CE marking confirms European construction product compliance. ISO 14001 certification confirms the facility meets internationally recognised environmental management standards — required for projects with sustainability procurement policies or regulated-market import conditions.

Application Environments

Warehouses and Logistics Centres

≥ 70 MPa compressive strength and ≤ 0.03 g abrasion resistance (Taber CS-17, 1000 cycles) withstand forklift traffic, pallet loads, and industrial cleaning. The warehouse floor ROI case rests on extended service intervals versus painted or untreated concrete floors.

Factory and Industrial Plant Floors

The chemical resistant quartz sand coating — resisting oils, fuels, dilute acids, and alkalis — reduces contamination risk in manufacturing environments. Available in 8 standard colours (HC51-011 to HC51-018) for production zone colour-coding in ISO-certified facilities.

Car Parks and Showrooms

The granite-speckle finish suits above-grade and underground car parks, showrooms, and retail spaces. Custom RAL/Pantone colour matching available beyond the 8 standard stocked colours.

epoxy-colored-sand-floor-coating-scene.png


Self-Leveling Industrial Flooring Installation

Correct self-leveling industrial flooring installation determines long-term surface performance. Five-stage process:

  • Substrate Preparation: Grind or shot-blast concrete to CSP 3–4. Repair cracks and voids. Inadequate preparation is the primary cause of bonding failure.
  • Primer Application: Apply epoxy primer; cure 4–8 hours at 20°C to seal the substrate and establish bond integrity.
  • Base Coat with Sand Broadcast: Apply epoxy base coat by roller; broadcast coloured quartz sand while wet to build texture and thickness.
  • Self-Leveling Topcoat: Mix two components at the specified ratio; spread with a notched squeegee and back-roll with a spiked roller to release entrapped air.
  • Curing: 24 hours before foot traffic; 7 days before vehicle traffic at 20°C.


Why Choose Us

  • 20 years of epoxy floor coating manufacturing with consistent two-component formulation quality
  • ISO 9001 & ISO 14001 certified; annual production capacity 11,000 tons
  • 8 standard colours in stock; custom RAL/Pantone colour matching available
  • MOQ 1 ton per colour; OEM/private label with custom 25kg packaging
  • Full documentation: CE certificate, COA, TDS, MSDS
  • Technical support for substrate assessment and application rate calculation

details (1).png

About Company

Shandong Dingtai Waterproof Technology Co., Ltd. is a leading manufacturer based in China' s largest waterproof material production hub-Taitou Industrial Park.As a company with independent import-export rights,we have successfully supplied products across global markets countriesand regions such as North America, Southeast Asia, South America, Africa,Europe and the Middle East. Our commitment to superior quality andreliable service has earned us a strong international reputation andgrowing market presence.

details (2).png

details (3).png

Frequently Asked Questions

Q1: Why choose us ?

A: We are professional manufacturer, and we can provide the best product ,competitive priceand excellent service.

Q2: Do you provide sample ?ls it free or extra ?

A: Yes,we can provide free sample for quality inspection.According to the regulations of our company , you should assume the freight ,and we will return the freight if you place the order.

Q3: How about the delivery time ?

A: 7-15 days after receive the deposit or LC at sight

Q4: How does your factory do regarding quality control?

A: Quality is priority,. We always attach great importance to quality control from the very beginning to the end. We have a professional QA/QC team to ensure the quality.

Q5: Do you accept OEM or ODM order?

A: Yes, we accept both OEM and ODM for customers.

Q6: What are your terms of delivery?

A: We can accept EXW, FOB, ClF, etc. You can choose one which is the most convenient for you.

Q7: What is the payment way?

A: TT, L/C at sight, West Union,Online Bank Payment.

Q8: Are you trading company or manufacturer?

A: We are manufacturer.So we have a lower price than trading company.

Epoxy Colored Sand Self-Leveling Floor Coating – Standard Grade, 25kg, 8 Colours

Standard grade epoxy colored sand self-leveling floor coating, 25kg bucket. Granite-effect speckled finish in 8 standard colours (HC51-011 to 018). Chemical resistant, wear resistant, seamless floor for factories, warehouses, and car parks. MOQ 1 ton. CE certified.

Request a Quote

You May Also Like

isoepoxy colored sand self leveling floor coating  standard grade 25kg 8 colours-1

Get a Free Quote

Our representative will contact you soon.
Email
Mobile/WhatsApp
Name
Company Name
Message
0/1000