20mm-self-adhesive-bitumen-waterproof-membrane-with-aluminum-foil--reflective-heat-resistant, 20mm-self-adhesive-bitumen-waterproof-membrane-with-aluminum-foil--reflective-heat-resistant, /self-adhesive-waterproof-membrane
2.0mm self-adhesive aluminum foil faced bitumen waterproof membrane. Highly reflective, UV-proof, heat-resistant — ideal for exposed roofing, ductwork, and HVAC insulation systems. Cold-applied, factory supply.
A reflective bitumen membrane is a modified bitumen waterproofing sheet with a bright aluminum foil laminated on its top surface. The foil reflects over 80% of incoming solar radiation, preventing the bituminous layer from absorbing heat and transferring it into the building below. This 2.0mm self-adhesive reflective bitumen membrane combines waterproofing performance with measurable thermal and UV protection in a single cold-applied system — making it the preferred cap sheet for exposed flat roofing in high-solar-radiation climates. Consider a logistics warehouse rooftop in a coastal Southeast Asian city: summer roof surface temperatures regularly exceed 70°C on standard black bitumen, driving up cooling loads for the entire facility. Specifying a reflective bitumen membrane with aluminum foil surface directly addresses that heat gain at source.
The aluminum foil surface of this reflective bitumen membrane reflects ≥ 80% of incident solar radiation. Where a conventional black bitumen cap sheet absorbs and re-radiates heat into the building, this solar reflective roof membrane keeps the roof surface 10–20°C cooler — cutting HVAC loads directly. For procurement teams in Southeast Asia, the Middle East, and other high-insolation markets, this 80% reflectivity is a test-verified figure, not a marketing claim. The reflective bitumen membrane specification is particularly effective in industrial and commercial buildings where cooling energy accounts for a significant share of operational costs.
UV oxidation is the primary aging mechanism in exposed bitumen membranes — it causes surface hardening, cracking, and premature failure. The aluminum foil of this reflective bitumen membrane acts as a complete physical UV shield, blocking all UV radiation from reaching the bituminous compound beneath. Unlike UV-inhibiting surface coatings that degrade over years of weathering, the foil barrier is permanent. This structural advantage of aluminum foil waterproofing over coated alternatives translates directly into longer service intervals and reduced lifecycle replacement costs.
This cold-applied waterproofing membrane uses a pressure-sensitive self-adhesive backing — installation is a peel-and-press process requiring no torch or heat equipment. In fire-restricted sites (occupied buildings, HVAC ductwork, facilities with flammable inventory), this cold application method eliminates safety compliance risk. Note that self-adhesive bonding requires a clean, dry, primed substrate for reliable adhesion; on rough or moisture-affected surfaces, a hot-applied system may achieve higher initial bond strength. The no-flame advantage of this reflective bitumen membrane is maximized when substrate preparation follows the product TDS.
The aluminum foil layer also functions as a vapor retarder. In cold-storage roofing, refrigerated warehouses, and high-humidity industrial buildings, this reflective bitumen membrane fulfills both the waterproofing layer and vapor control layer roles in a single product — eliminating the need for a separate vapor retarder in the roof assembly and reducing total installed material cost. This dual function is especially valuable where roof assembly depth and layer count are constrained by project design requirements.
The aluminum foil laminate is food-grade, maintaining chemical stability under acid rain, industrial fumes, and salt spray. For coastal industrial plants and chemical manufacturing facilities, this prevents foil delamination that would compromise both the UV barrier and reflective functions of the membrane over time.
| Parameter | Value |
| Modifier | SBS / APP |
| Reinforcement | Polyester mat |
| Total Thickness | 2.0mm |
| Top Surface | Aluminum foil (0.08mm–0.12mm) |
| Solar Reflectivity | ≥ 80% |
| Roll Size | 1m × 15m (customizable) |
| Peel Adhesion | ≥ 1.5 N/mm |
| Tensile Strength | ≥ 500 N/50mm |
| Low-Temp Flexibility | -20°C (SBS) / -5°C (APP) |
| Heat Resistance | 90°C (SBS) / 130°C (APP) |
| Water Tightness | 0.3 MPa, 120 min |
All parameters are sourced from product specification data and batch test certificates available upon request.
Both grades of this reflective bitumen membrane use identical aluminum foil surface, roll dimensions, and self-adhesive backing. The modifier selection is climate-driven: SBS provides elastic recovery and -20°C low-temperature flexibility for cold-climate and high-cycling environments; APP delivers 130°C heat resistance and greater UV stability within the bituminous compound for consistently hot climates. International procurement teams sourcing SBS/APP modified bitumen waterproofing for multi-region projects can order both grades from the same factory under consistent quality and foil specification.
This reflective bitumen membrane is designed as a cap sheet for exposed flat roof systems with no overlay protection layer. It is suited to factory rooftops, warehouses, distribution centers, and commercial buildings in warm-climate markets. Contractors sourcing a reflective bitumen membrane for tropical or subtropical projects should specify the APP-modified grade (130°C heat resistance) rather than standard SBS — a mismatched grade is a common cause of surface softening and flow distortion on high-heat rooftops. The SBS grade (-20°C flexibility) remains the correct specification for cold-climate or high thermal-cycling applications.
Beyond roofing, the self-adhesive backing and aluminum foil surface make this reflective bitumen membrane well-suited for insulation wrapping on HVAC ductwork, refrigeration pipework, and mechanical plant enclosures. For cold-storage facility roofing specifically, the combination of solar reflectivity, vapor barrier function, and SBS low-temperature flexibility (-20°C) addresses three core technical requirements in a single product layer, reducing system complexity and supplier count for procurement teams managing multi-component roof specifications.


Shandong Dingtai Waterproof Technology Co., Ltd. is a leading manufacturer based in China' s largest waterproof material production hub-Taitou Industrial Park.As a company with independent import-export rights,we have successfully supplied products across global markets countriesand regions such as North America, Southeast Asia, South America, Africa,Europe and the Middle East. Our commitment to superior quality andreliable service has earned us a strong international reputation andgrowing market presence.

Q1: Why choose us ?
A: We are professional manufacturer, and we can provide the best product ,competitive priceand excellent service.
Q2: Do you provide sample ?ls it free or extra ?
A: Yes,we can provide free sample for quality inspection.According to the regulations of our company , you should assume the freight ,and we will return the freight if you place the order.
Q3: How about the delivery time ?
A: 7-15 days after receive the deposit or LC at sight
Q4: How does your factory do regarding quality control?
A: Quality is priority,. We always attach great importance to quality control from the very beginning to the end. We have a professional QA/QC team to ensure the quality.
Q5: Do you accept OEM or ODM order?
A: Yes, we accept both OEM and ODM for customers.
Q6: What are your terms of delivery?
A: We can accept EXW, FOB, ClF, etc. You can choose one which is the most convenient for you.
Q7: What is the payment way?
A: TT, L/C at sight, West Union,Online Bank Payment.
Q8: Are you trading company or manufacturer?
A: We are manufacturer.So we have a lower price than trading company.
2.0mm self-adhesive aluminum foil faced bitumen waterproof membrane. Highly reflective, UV-proof, heat-resistant — ideal for exposed roofing, ductwork, and HVAC insulation systems. Cold-applied, factory supply.