anti-static-epoxy-floor-paint--25kg-a21kg--b4kg-esd-floor-for-electronics--data-centres, anti-static-epoxy-floor-paint--25kg-a21kg--b4kg-esd-floor-for-electronics--data-centres, /floor-paint
Inquiry
anti-static-epoxy-floor-paint--25kg-a21kg--b4kg-esd-floor-for-electronics--data-centres, anti-static-epoxy-floor-paint--25kg-a21kg--b4kg-esd-floor-for-electronics--data-centres, 
Inquiry

Anti-Static Epoxy Floor Paint – 25kg (A:21kg + B:4kg), ESD Floor for Electronics & Data Centres

Anti-static epoxy floor paint, 25kg set (A 21kg + B 4kg). Surface resistance 10⁶–10⁹ Ω — ESD compliant floor for electronics manufacturing, data centres, and precision instrument facilities. 16 colours. MOQ 1 ton. CE certified.

Request a Quote
  • Overview

Overview

ESD Floor Paint Comparison: What Your Facility Needs to Evaluate

Many procurement teams begin an ESD floor paint comparison by lining up supplier quotes — and only discover months later that the real cost gap shows up in re-testing, re-coating, or compliance failures. Think of an anti-static floor coating like a resistor in a circuit: it has to slow electrostatic charge into a controlled, dissipative range. Get the resistance window wrong, and even an expensive coating becomes a liability.

This Anti-Static Epoxy Floor Paint achieves a verified surface resistance of 10⁶–10⁹ Ω — the electrostatic dissipative (ESD) classification defined under EN 61340-5-1 and ANSI/ESD S20.20. Conductivity is delivered by a conductive carbon additive integral to the epoxy film, not a surface treatment. The ESD performance does not wear away with foot traffic, fork-lift passes, or cleaning cycles.

img-msspfktr-ca3df005.png

Key Features

Permanent, Integral Anti-Static Performance

Conductivity is built into the epoxy film through a precisely loaded conductive carbon additive — not applied as a topical treatment. No periodic retreatment schedule, no risk of uneven ESD degradation. For facilities that have seen topical anti-static treatments lose effectiveness after cleaning, this is the structural difference that matters in a conductive epoxy floor implementation. The resistance remains stable across the coating's full service life.

EN 61340-5-1 / ANSI/ESD S20.20 Compliance with Full Documentation

As an EN 61340-5-1 certified supplier, we provide: CE certificate, EN 61340-5-1 test reports, COA, TDS, and MSDS. Selecting ESD coatings without reviewing actual test reports is a common procurement error. Process verification — not brand trust — is the reliable path to compliance confidence before facility commissioning.

Grounding System Compatibility

This product is designed for use with copper grounding strips and earth bonding systems. A complete ESD floor system — primer, anti-static topcoat, and grounding specification — is available. A conductive epoxy floor implementation without a properly designed grounding path will not protect against ESD events regardless of coating resistance. The floor coating and the grounding system must work together.

Full 16-Colour Range Without Compromising ESD Performance

All 16 HC51 series colours — Light Grey, Medium Grey, Dark Grey, Beige, Light Green, Blue-Grey, Racing Red, and more — are available at the same surface resistance specification. Colour-coded zone layouts are a standard requirement in semiconductor cleanroom flooring and electronics manufacturing facilities; anti-static performance does not restrict colour selection in this product line.

High Mechanical Durability

Compressive strength ≥ 60 MPa and tensile bond strength ≥ 1.5 MPa suit the mechanical demands of electronics manufacturing floors, data centre surrounds, and cleanroom environments with steady equipment movement and rigorous cleaning regimens.

Core Technical Specifications

Parameter Value
Product Type Two-component anti-static epoxy floor paint
Mix Ratio (by weight) Component A : Component B = 21 : 4
Packaging 25 kg/set (A: 21 kg + B: 4 kg)
Surface Resistance 10⁶–10⁹ Ω (EN 61340-5-1 electrostatic dissipative range)
Compressive Strength ≥ 60 MPa
Tensile Bond Strength ≥ 1.5 MPa
Dry Film Thickness 0.2–0.4 mm per coat (2 coats)
Application Rate 0.2–0.3 kg/m² per coat
Standard Colours 16 colours (HC51 series)
MOQ 1 tonne
Certifications CE, ISO 9001, ISO 14001

Any serious ESD floor paint comparison starts with the resistance specification. EN 61340-5-1 defines three zones: conductive (<10⁶ Ω), electrostatic dissipative (10⁶–10⁹ Ω), and insulative (>10¹² Ω). Facilities handling sensitive electronic components or operating semiconductor cleanroom flooring need the dissipative range — verified by test report, not assumed from a supplier brochure.

Application Scenarios

Electronics and Semiconductor Manufacturing

Specifying semiconductor cleanroom flooring for a wafer fabrication bay means the coating must meet ANSI/ESD S20.20, provide a consistent dissipative surface, and integrate with the facility grounding plan. Anti-static epoxy ROI case studies show that facilities choosing certified, integral-conductivity coatings avoided re-coating cycles that inflate total floor ownership cost over five years — the comparison is not just about upfront price per square metre. Facilities that invest in compliant documentation upfront also avoid costly re-certification during periodic ESD audits.

Data Centres and Server Rooms

Raised floors and concrete subfloors both present ESD risks during hardware installation and maintenance. A conductive epoxy floor implementation in a data centre should achieve 10⁶–10⁹ Ω under site ambient conditions — temperature and humidity both affect measured resistance. If your facility operates at low relative humidity (below 30%), verifying resistance under those specific conditions is important. Coatings with integral carbon loading maintain more consistent resistance across humidity variation than topical treatments.

Pharmaceutical Cleanrooms and Precision Instrument Workshops

Pharmaceutical cleanroom floors require both contamination control and ESD protection simultaneously. The smooth solid-colour finish supports standard cleaning protocols; integral anti-static performance reduces the secondary contamination risk associated with topical anti-static sprays applied during production. For precision instrument assembly workshops, a permanent dissipative surface that does not require additional chemical treatments during production operations simplifies the maintenance schedule.

floor-paint-scene.png


Why Choose Us

  • 20 years of anti-static epoxy floor coating manufacturing; ESD performance verified by independent test
  • ISO 9001 & ISO 14001 certified; consistent carbon additive loading for reliable surface resistance across batches
  • Complete ESD floor system supply: primer + anti-static coat + copper grounding strip specification
  • 16 standard colours; custom resistance range (10⁵–10¹⁰ Ω) on request
  • Full documentation: CE, EN 61340-5-1 test reports, COA, TDS, MSDS
  • Technical support for ESD system design and grounding layout specification

details (1).png

About Company

Shandong Dingtai Waterproof Technology Co., Ltd. is a leading manufacturer based in China' s largest waterproof material production hub-Taitou Industrial Park.As a company with independent import-export rights,we have successfully supplied products across global markets countriesand regions such as North America, Southeast Asia, South America, Africa,Europe and the Middle East. Our commitment to superior quality andreliable service has earned us a strong international reputation andgrowing market presence.

details (2).png

details (3).png

Frequently Asked Questions

Q1: Why choose us ?

A: We are professional manufacturer, and we can provide the best product ,competitive priceand excellent service.

Q2: Do you provide sample ?ls it free or extra ?

A: Yes,we can provide free sample for quality inspection.According to the regulations of our company , you should assume the freight ,and we will return the freight if you place the order.

Q3: How about the delivery time ?

A: 7-15 days after receive the deposit or LC at sight

Q4: How does your factory do regarding quality control?

A: Quality is priority,. We always attach great importance to quality control from the very beginning to the end. We have a professional QA/QC team to ensure the quality.

Q5: Do you accept OEM or ODM order?

A: Yes, we accept both OEM and ODM for customers.

Q6: What are your terms of delivery?

A: We can accept EXW, FOB, ClF, etc. You can choose one which is the most convenient for you.

Q7: What is the payment way?

A: TT, L/C at sight, West Union,Online Bank Payment.

Q8: Are you trading company or manufacturer?

A: We are manufacturer.So we have a lower price than trading company.

Anti-Static Epoxy Floor Paint – 25kg (A:21kg + B:4kg), ESD Floor for Electronics & Data Centres

Anti-static epoxy floor paint, 25kg set (A 21kg + B 4kg). Surface resistance 10⁶–10⁹ Ω — ESD compliant floor for electronics manufacturing, data centres, and precision instrument facilities. 16 colours. MOQ 1 ton. CE certified.

Request a Quote

You May Also Like

anti static epoxy floor paint  25kg a21kg  b4kg esd floor for electronics  data centres-1

Get a Free Quote

Our representative will contact you soon.
Email
Mobile/WhatsApp
Name
Company Name
Message
0/1000