bitumen-waterproof-tape--12mm-pe-film-surface-custom-width--length, bitumen-waterproof-tape--12mm-pe-film-surface-custom-width--length, /bitumen-waterproof-tape
Inquiry
bitumen-waterproof-tape--12mm-pe-film-surface-custom-width--length, bitumen-waterproof-tape--12mm-pe-film-surface-custom-width--length, 
Inquiry

Bitumen Waterproof Tape – 1.2mm, PE Film Surface, Custom Width & Length

Factory-direct bitumen waterproof tape, 1.2mm thick, PE film surface. Self-adhesive modified bitumen sealing tape for roof seams, pipe penetrations, flashing details, and joint waterproofing. Width 50–300mm, length 7.5–20m, custom. CE certified.

Request a Quote
  • Overview

Overview

Bitumen Waterproof Tape – 1.2mm SBS Modified, PE Film Surface

This 1.2mm Bitumen Waterproof Tape with PE Film Surface is a self-adhesive sealing strip manufactured from SBS-modified bitumen compound with a smooth PE film top surface and a silicone-coated release liner. It delivers an instant, watertight seal through a straightforward peel-and-press process: no open flame, no primer, no specialist equipment. Supplied in widths from 50mm to 300mm and roll lengths from 7.5m to 20m — fully customizable — this SBS modified bitumen tape is engineered for joint sealing, seam reinforcement, and penetration detail waterproofing where a thin, conformable, self-adhesive bitumen strip is needed on prepared substrates.

Bitumen Waterproof Tape – 1.2mm, PE Film Surface, Custom Width & Length details

Key Features

Peel-and-Press Self-Adhesive — No Flame Required

The self-adhesive modified bitumen adhesive bonds to concrete, masonry, metal flashing, and existing membranes upon pressing. No flame, no primer, no hot-work equipment. This bitumen waterproof tape is well suited to fire-restricted sites and enclosed spaces where hot-applied systems are impractical. For best adhesion, apply to a clean, dry substrate; on rough or damp surfaces, surface preparation or priming is recommended before installation to ensure a reliable initial bond.

SBS-Modified Bitumen — Cold-Climate Flexibility

The SBS modifier delivers low-temperature flexibility to -20°C, keeping the tape pliable and adhesive in cold-climate construction conditions. SBS-modified bitumen is the dominant modifier in high-performance waterproofing membranes globally. Specifying this SBS modified bitumen tape for detail work brings the same proven chemical technology to seams and joints that your primary membrane system relies on, ensuring material compatibility throughout the waterproofing assembly.

PE Film Top Surface — Overlay Compatible

The smooth PE film top surface is compatible with mortar, screed, tile adhesive, and cementitious overlay systems applied over it — suitable for buried or concealed details such as parapet base flashing, pipe collar coverups, and construction joints that will be tiled over. The PE film resists cement alkalinity and bonds with standard overlay adhesives, making this tape a practical choice within composite waterproofing build-ups.

Custom Width Roofing Tape — Matched to Project Requirements

Standard widths: 50–300mm; custom widths available up to 1000mm. Roll lengths: 7.5–20m, customizable. This custom width roofing tape option minimizes on-site cutting waste: 75mm matches standard seam lap widths; 100mm covers most pipe collar details; wider formats address structural joint flashing. Ordering to required dimensions reduces surplus or shortfall, keeping project material quantities accurate and procurement straightforward.

Technical Specifications

Parameter Value
Modifier SBS modified bitumen
Top Surface PE film
Release Liner Silicone-coated film
Thickness 1.2mm
Width Range 50–300mm (custom up to 1000mm)
Roll Length 7.5–20m (customizable)
Peel Adhesion ≥ 1.2 N/mm
Tensile Strength ≥ 300 N/50mm
Low-Temperature Flexibility -20°C
Water Tightness Pass at 0.3 MPa
Certifications CE, ISO 9001, ISO 14001

Performance benchmarks — peel adhesion ≥1.2 N/mm, tensile strength ≥300 N/50mm, water tightness at 0.3 MPa — are real, testable values from the product TDS. CE certified waterproofing documentation is available alongside COA, TDS, and MSDS, supporting international procurement compliance requirements across European and other regulated markets.

Application Scenarios

Roof Membrane Seam Sealing

In flat and low-slope roofing systems, lap seams between primary membrane sheets are frequent failure points in the overall waterproofing assembly. This bitumen waterproof tape reinforces seams and provides a secondary seal when applied with adequate overlap on both membrane surfaces. It is particularly useful for seam repairs on existing systems, transition details where a primary membrane meets metal flashing, and temporary weatherproofing during phased construction. The custom width roofing tape format allows precise matching to required seam coverage width, reducing installation adjustment on site.

Pipe and Duct Penetration Collar Waterproofing

Pipe penetrations through waterproof decks create joints that sheet membranes alone cannot easily seal. This self-adhesive bitumen tape applied in overlapping segments around the pipe collar and onto the surrounding deck forms a conformable seal without cutting sheet material. For standard pipe penetrations in the 50–150mm diameter range, a 75–150mm tape width provides adequate overlap and manageable installation. Ensure the substrate around the penetration is clean and dry before applying the tape.

Concrete Construction Joint Sealing

Construction joint sealing in foundation slabs, podium connections, and wall-to-slab transitions requires a tape that bridges the joint and bonds to concrete before cover layers are placed. The peel-and-press format works well here: the joint surface is typically accessible and controllable during the installation window. For movement joints, a wider tape width with centrally positioned coverage provides better bridging performance and accommodates minor displacement. Construction joint sealing is a core use case this bitumen waterproof tape addresses directly, and the CE certified waterproofing credentials support its use in formal project specification and compliance documentation.

bitumen-waterproof-tape-scene.png

Why Choose Us

  • 20 years of modified bitumen waterproof tape manufacturing with consistent adhesive quality
  • ISO 9001 & ISO 14001 certified; wide range of widths and lengths available from stock or custom order
  • Custom width (50–1000mm), thickness (1.2–2.0mm), and roll length (7.5–20m) to specification
  • MOQ flexible — suitable for both project and distributor supply
  • Full documentation: CE certificate, COA, TDS, MSDS
  • OEM/private label packaging available

details (1).png

About Company

Shandong Dingtai Waterproof Technology Co., Ltd. is a leading manufacturer based in China' s largest waterproof material production hub-Taitou Industrial Park.As a company with independent import-export rights,we have successfully supplied products across global markets countriesand regions such as North America, Southeast Asia, South America, Africa,Europe and the Middle East. Our commitment to superior quality andreliable service has earned us a strong international reputation andgrowing market presence.

details (2).png

details (3).png

Frequently Asked Questions

Q1: Why choose us ?

A: We are professional manufacturer, and we can provide the best product ,competitive priceand excellent service.

Q2: Do you provide sample ?ls it free or extra ?

A: Yes,we can provide free sample for quality inspection.According to the regulations of our company , you should assume the freight ,and we will return the freight if you place the order.

Q3: How about the delivery time ?

A: 7-15 days after receive the deposit or LC at sight

Q4: How does your factory do regarding quality control?

A: Quality is priority,. We always attach great importance to quality control from the very beginning to the end. We have a professional QA/QC team to ensure the quality.

Q5: Do you accept OEM or ODM order?

A: Yes, we accept both OEM and ODM for customers.

Q6: What are your terms of delivery?

A: We can accept EXW, FOB, ClF, etc. You can choose one which is the most convenient for you.

Q7: What is the payment way?

A: TT, L/C at sight, West Union,Online Bank Payment.

Q8: Are you trading company or manufacturer?

A: We are manufacturer.So we have a lower price than trading company.

Bitumen Waterproof Tape – 1.2mm, PE Film Surface, Custom Width & Length

Factory-direct bitumen waterproof tape, 1.2mm thick, PE film surface. Self-adhesive modified bitumen sealing tape for roof seams, pipe penetrations, flashing details, and joint waterproofing. Width 50–300mm, length 7.5–20m, custom. CE certified.

Request a Quote

You May Also Like

bitumen waterproof tape  12mm pe film surface custom width  length-1

Get a Free Quote

Our representative will contact you soon.
Email
Mobile/WhatsApp
Name
Company Name
Message
0/1000