butyl-self-adhesive-waterproof-membrane--12mm-standard-grade-pe-film-surface-1m--20m, butyl-self-adhesive-waterproof-membrane--12mm-standard-grade-pe-film-surface-1m--20m, /butyl-self-adhesive-waterproof-membrane
1.2mm standard grade butyl rubber self-adhesive waterproof membrane with PE film surface. High tensile strength, superior elongation, and reliable cold-applied waterproofing for roofing, underground basements, tunnels, and bridge decks. CE and ISO 14001 certified. Factory direct.
When a waterproofing system fails below grade, finding the source is often costlier than the repair. Conventional loose-laid membranes allow water to travel beneath an unbonded layer, hiding the entry point until structural damage spreads. The 1.2mm Standard Grade Butyl Self-Adhesive Waterproof Membrane addresses this at the system level: its permanently pressure-sensitive adhesive bonds directly to the primed substrate, creating a fully bonded sealed barrier from installation day one. Leaks are more readily localised and traceable — a critical advantage for basement, tunnel, and bridge deck applications where remediation access is limited and expensive.
This butyl waterproof membrane is the standard specification grade in our range, balancing tensile strength, elongation, and cost-efficiency across roofing and civil engineering applications. CE certified waterproofing documentation and third-party test data support specification submissions where performance traceability is required.
The permanently pressure-sensitive adhesive forms complete contact with the primed concrete substrate, eliminating unattached zones where water migrates in loose-laid systems. Peel adhesion of ≥ 1.5 N/mm on primed concrete holds under both positive and negative hydrostatic pressure, making this butyl waterproof membrane suitable for high water-table basement and tunnel environments.
At ≥ 500% elongation at break, the butyl rubber compound can bridge substrate cracks up to approximately 5mm — qualifying this as a genuine crack-bridging membrane. Thermal cycling, structural settlement, and vibration-induced movement are absorbed without membrane failure. Bituminous torch-on materials typically achieve 30–50% elongation; appropriate for stable substrates, but less suited for structures where long-term movement is expected.
CE marking under the Construction Products Regulation (CPR) requires testing and a Declaration of Performance (DoP) covering tensile strength, elongation, water tightness, and adhesion. This butyl waterproof membrane carries CE certification, with full documentation available on request. For European project specifications, public tenders, or EN-standard-referenced procurement, CE certified waterproofing records help address the compliance transparency gap common in cross-border sourcing.
As an ISO 14001 roofing supplier, our facility operates under a certified environmental management system with documented procedures for waste reduction, chemical handling, and emissions monitoring. This supports LEED, BREEAM, and green building programme requirements, and signals the manufacturing consistency that matters in large, multi-delivery infrastructure contracts.
Peel-and-stick installation eliminates LPG torch equipment, reducing fire risk in confined underground spaces, occupied buildings, and hot-work-restricted sites. A practical note: cold-applied adhesion is temperature-sensitive. Below approximately 5°C, initial tack strength decreases; a low-temperature primer or substrate pre-warming is recommended to maintain the full ≥ 1.5 N/mm adhesion specification. The –40°C to +70°C operating range covers cold-storage roofing, high-altitude tunnels, and hot-climate flat roofing within a single product specification.
| Parameter | Value |
|---|---|
| Adhesive | Synthetic butyl rubber |
| Top Surface | PE (Polyethylene) film |
| Release Liner | Silicone-coated film |
| Thickness | 1.2mm |
| Standard Roll Size | 1.0m × 20m |
| Customizable Width | 0.5m – 2.0m |
| Customizable Length | 10m – 100m |
| Peel Adhesion (primed concrete) | ≥ 1.5 N/mm |
| Tensile Strength | ≥ 200 N/50mm |
| Elongation at Break | ≥ 500% |
| Low-Temperature Flexibility | –40°C |
| Heat Resistance | 70°C |
| Water Tightness | Pass at 0.4 MPa, 30 min |
| Certification | CE, ISO 14001 |
This membrane functions as a primary underground waterproofing solution on horizontal slabs and vertical walls. Water tightness at 0.4 MPa for 30 minutes corresponds to approximately 40 metres of water head — covering most civil basement, cut-and-cover tunnel, and deep-foundation applications. On retaining walls, the self-adhesive layer is applied to prepared concrete and protected with a drainage board before backfill, forming a below-grade waterproofing system resistant to construction-phase and in-service hydrostatic loading.
On flat and low-slope roofs, the PE film surface is compatible with protection boards and ballasted overlay systems. In bridge deck applications under asphalt wearing courses, the crack-bridging membrane accommodates deck flexure from live loads and thermal expansion. The combination of ≥ 500% elongation and ≥ 200 N/50mm tensile strength helps maintain waterproof integrity under shear and dynamic loading conditions on road and railway infrastructure.


Shandong Dingtai Waterproof Technology Co., Ltd. is a leading manufacturer based in China' s largest waterproof material production hub-Taitou Industrial Park.As a company with independent import-export rights,we have successfully supplied products across global markets countriesand regions such as North America, Southeast Asia, South America, Africa,Europe and the Middle East. Our commitment to superior quality andreliable service has earned us a strong international reputation andgrowing market presence.

Q1: Why choose us ?
A: We are professional manufacturer, and we can provide the best product ,competitive priceand excellent service.
Q2: Do you provide sample ?ls it free or extra ?
A: Yes,we can provide free sample for quality inspection.According to the regulations of our company , you should assume the freight ,and we will return the freight if you place the order.
Q3: How about the delivery time ?
A: 7-15 days after receive the deposit or LC at sight
Q4: How does your factory do regarding quality control?
A: Quality is priority,. We always attach great importance to quality control from the very beginning to the end. We have a professional QA/QC team to ensure the quality.
Q5: Do you accept OEM or ODM order?
A: Yes, we accept both OEM and ODM for customers.
Q6: What are your terms of delivery?
A: We can accept EXW, FOB, ClF, etc. You can choose one which is the most convenient for you.
Q7: What is the payment way?
A: TT, L/C at sight, West Union,Online Bank Payment.
Q8: Are you trading company or manufacturer?
A: We are manufacturer.So we have a lower price than trading company.