js-polymer-cement-waterproof-coating--type-i-flexible-grade-20kg-swimming-pool--wet-room, js-polymer-cement-waterproof-coating--type-i-flexible-grade-20kg-swimming-pool--wet-room, /polymer-cement-basedjs-waterproof-coating
Inquiry
js-polymer-cement-waterproof-coating--type-i-flexible-grade-20kg-swimming-pool--wet-room, js-polymer-cement-waterproof-coating--type-i-flexible-grade-20kg-swimming-pool--wet-room, 
Inquiry

JS Polymer Cement Waterproof Coating – Type I Flexible Grade, 20kg, Swimming Pool & Wet Room

Type I flexible JS polymer cement waterproof coating, 20kg. High polymer-to-cement ratio delivers elongation ≥ 200% — ideal for swimming pools, wet rooms, and substrates with movement. Two-component, brush or roller applied. MOQ 1 ton. CE certified.

Request a Quote
  • Overview

Overview

JS Waterproof Coating Comparison: Grade Selection Guide

A rigorous JS waterproof coating comparison starts with grade selection, not price. The fundamental choice — Type I flexible versus Type II rigid — determines whether the coating will hold through the substrate movement cycles your application demands. Selecting the wrong grade leads to premature failure and remedial costs that exceed the original material spend many times over.

JS Polymer Cement Waterproof Coating – Type I Flexible Grade, 20kg, Swimming Pool & Wet Room supplier

What Is JS Polymer Cement Waterproof Coating?

JS polymer cement waterproof coating is a two-component system: a polymer liquid (Component A) mixed with cement powder (Component B) at the application site. Think of it as reinforced concrete in coating form — cement bonds to mineral substrates and resists alkalinity, while the polymer network delivers the elasticity that pure cementitious coatings lack. The "JS" designation originates from GB/T 23445, China's national standard for polymer-cement composite waterproof coatings, which classifies the product into Type I (flexible) and Type II (rigid) based on elongation performance.

Key Performance Features

Elongation at Break ≥ 200%

The Type I formulation's elevated polymer-to-cement ratio delivers elongation exceeding 200%. To be precise, this is confirmed under GB/T 23445 test conditions; when evaluating datasheets across a JS waterproof coating comparison, always verify the test standard used, since values from different protocols are not directly comparable. In practice, this elasticity bridges active cracks up to 2 mm and absorbs differential movement between concrete, tile adhesive, and finish layers over the building lifecycle.

Bond Strength and Positive/Negative Application

Bond strength of ≥ 0.5 MPa to concrete and masonry resists delamination under hydrostatic pressure from either face. The coating applies to both water-facing (positive) and non-water-facing (negative/blind) sides — a significant advantage in retrofit projects where access to the positive face is restricted: in-use swimming pools, existing basement walls, and underground cisterns.

CE Certification and GB/T 23445 Compliance

The dual compliance profile directly reduces procurement friction for international buyers. CE certification supports EU market acceptance; GB/T 23445 Type I certification confirms Chinese national standard compliance. As a CE certified waterproof coating supplier, the manufacturer provides CE certificate, GB/T 23445 test report, COA, TDS, and MSDS. This documentation package resolves the most common cross-standard compliance pain point: opacity of Chinese supplier certifications relative to target-market requirements.

Potable Water Safety

This product carries potable water safety certification, qualifying it for drinking water reservoirs and swimming pools subject to water-contact health standards. Omitting this certification to reduce unit cost can trigger regulatory compliance failures at project handover — consequences that exceed the material cost saving.

Type I vs. Type II: JS Waterproof Coating Comparison

Parameter Type I (Flexible) Type II (Rigid)
Elongation at Break ≥ 200% ≥ 80%
Tensile Strength ≥ 1.2 MPa ≥ 1.8 MPa
Crack-Bridging Up to 2 mm active cracks Hairline cracks only
Best Suited For Movement, vibration, thermal cycling Stable, rigid substrates
Standard GB/T 23445 Type I GB/T 23445 Type II

If your substrate moves, vibrates, or experiences thermal cycling — swimming pools, wet room floors, roof decks with active cracking — specify Type I. Using Type II in a high-movement application is a common specification error whose cost only appears after the coating fails and remediation begins.

Technical Specifications

Parameter Value
Type Two-component JS polymer cement, Type I flexible
Liquid:Powder Mix Ratio Approx. 1:0.4–0.5 (by weight)
Elongation at Break ≥ 200%
Tensile Strength ≥ 1.2 MPa
Bond Strength to Concrete ≥ 0.5 MPa
Water Tightness Pass at 0.3 MPa, 30 min
Application Rate 1.5–2.0 kg/m² (2 coats)
Packaging 20 kg/set (liquid + powder)
MOQ 1 ton
Certification CE, ISO 14001
Standard GB/T 23445 Type I


Application Scenarios

Polymer Cement Waterproofing for Swimming Pools

Polymer cement waterproofing for swimming pools demands high elongation performance. Pool shells endure constant hydrostatic pressure, chlorine exposure, and thermal expansion cycles — conditions that cause rigid coatings to crack within a few seasons. The ≥ 200% elongation of the Type I grade sustains waterproof integrity through these cycles. The potable water safety certification ensures compliance with health standards for bather contact.

Wet Rooms, Bathrooms, and Roof Decks

Wet room substrates move under temperature and humidity cycles; tile adhesive and concrete expand and contract at different rates, generating differential movement a rigid coating cannot handle. Roof decks in climates with significant day-night temperature variation experience millimeter-scale expansion and contraction across diurnal cycles — a coating without adequate elongation develops hairline fractures that progressively admit water. The Type I Flexible Grade addresses both these scenarios.

waterproof-coating-scene.png

Why Choose Us

  • 20 years of JS waterproof coating manufacturing with proven two-component formulation expertise
  • ISO 9001 & ISO 14001 certified; annual production capacity 11,000 tons
  • Liquid/powder ratio and polymer content adjustable to project elongation requirements
  • MOQ 1 ton; OEM/private label with custom colour and 20kg packaging
  • Full documentation: CE certificate, GB/T 23445 test report, COA, TDS, MSDS
  • Potable water safety certification available on request

details (1).png

About Company

Shandong Dingtai Waterproof Technology Co., Ltd. is a leading manufacturer based in China' s largest waterproof material production hub-Taitou Industrial Park.As a company with independent import-export rights,we have successfully supplied products across global markets countriesand regions such as North America, Southeast Asia, South America, Africa,Europe and the Middle East. Our commitment to superior quality andreliable service has earned us a strong international reputation andgrowing market presence.

details (2).png

details (3).png

Frequently Asked Questions

Q1: Why choose us ?

A: We are professional manufacturer, and we can provide the best product ,competitive priceand excellent service.

Q2: Do you provide sample ?ls it free or extra ?

A: Yes,we can provide free sample for quality inspection.According to the regulations of our company , you should assume the freight ,and we will return the freight if you place the order.

Q3: How about the delivery time ?

A: 7-15 days after receive the deposit or LC at sight

Q4: How does your factory do regarding quality control?

A: Quality is priority,. We always attach great importance to quality control from the very beginning to the end. We have a professional QA/QC team to ensure the quality.

Q5: Do you accept OEM or ODM order?

A: Yes, we accept both OEM and ODM for customers.

Q6: What are your terms of delivery?

A: We can accept EXW, FOB, ClF, etc. You can choose one which is the most convenient for you.

Q7: What is the payment way?

A: TT, L/C at sight, West Union,Online Bank Payment.

Q8: Are you trading company or manufacturer?

A: We are manufacturer.So we have a lower price than trading company.

JS Polymer Cement Waterproof Coating – Type I Flexible Grade, 20kg, Swimming Pool & Wet Room

Type I flexible JS polymer cement waterproof coating, 20kg. High polymer-to-cement ratio delivers elongation ≥ 200% — ideal for swimming pools, wet rooms, and substrates with movement. Two-component, brush or roller applied. MOQ 1 ton. CE certified.

Request a Quote

You May Also Like

js polymer cement waterproof coating  type i flexible grade 20kg swimming pool  wet room-1

Get a Free Quote

Our representative will contact you soon.
Email
Mobile/WhatsApp
Name
Company Name
Message
0/1000