js-polymer-cement-waterproof-coating--type-ii-semi-rigid-grade-20kg-general-purpose, js-polymer-cement-waterproof-coating--type-ii-semi-rigid-grade-20kg-general-purpose, /polymer-cement-basedjs-waterproof-coating
Type II semi-rigid JS polymer cement waterproof coating, 20kg. Balanced polymer-cement ratio for general-purpose waterproofing — rooftops, underground basements, foundations, and civil structures. High bond strength. MOQ 1 ton. CE certified.
In any JS waterproof coating comparison, Type II Semi-Rigid Grade is a widely-used benchmark — the grade that covers most construction waterproofing requirements. Think of JS coating types like load ratings on structural cable: the middle grade balances flexibility, bond strength, and cost in a way the extremes cannot. Manufactured by Shandong Dingtai Waterproof Technology Co., Ltd. to GB/T 23445 Type II, it occupies the midpoint between high-flexibility Type I and high-rigidity Type III.
Elongation ≥ 80% accommodates substrate cracking and thermal movement. Higher cement ratio versus Type I improves compressive strength for moderate-load and pedestrian-traffic surfaces. In a direct JS waterproof coating comparison, this balance removes the need to trade flexibility for structural performance on general construction applications.
Water tightness confirmed at 0.4 MPa for 30 minutes provides hydrostatic resistance waterproofing for basement walls, underground car parks, and civil structures under sustained groundwater pressure. The higher cement content versus Type I is the material basis for this performance advantage — making Type II suitable beyond exposed rooftops.
Bonds to concrete, masonry, cement mortar, and mineral substrates at ≥ 0.6 MPa. Compatible with tile adhesive, screed, and finish layers, reducing delamination risk in multi-layer assemblies. For construction waterproofing supplier qualification, this broad compatibility cuts the primers and transition materials required per project.
Brush, roller, or spray application works across flat areas, complex geometry, and detail work. The 2–3 coat system at 2.0–2.5 kg/m² supports staged application. No open-flame equipment required.
CE certificate, GB/T 23445 test report, COA, TDS, and MSDS available without lead-time delay — a consistent supply-chain advantage for international procurement requiring documented GB/T 23445 compliance. Standard parameters align with equivalent standards in Asian and Middle Eastern markets.
Meaningful Type II ROI analysis extends beyond unit price. Waterproofing failure remediation — stripping, substrate repair, re-application, schedule disruption — typically costs multiples of the original material budget. The real comparison for any construction waterproofing supplier evaluation is probability-weighted total project cost over a realistic service life. Type II's specification alignment with general construction needs eliminates the hidden cost of mis-specification: not over-engineered for rooftops, not under-specified for basements. For 5-ton-plus purchases, factory-direct pricing is available from Shandong Dingtai's 10,000-ton-capacity plant, ISO 9001 certified for batch-to-batch quality consistency.
Construction waterproofing supplier evaluation criteria: Is this a core product or catalog listing? Can supply sustain multi-phase project schedules? Is documentation audit-ready? For Shandong Dingtai, Type II is the highest-volume JS product — consistent raw material sourcing, 15 years of formulation experience, and Shandong production-cluster logistics support delivery continuity. MOQ 1 ton; OEM and private label available. Lead time: 7–15 days after deposit or L/C at sight. Payment: TT, L/C, online transfer. Full export documentation ready on request.
The question is not just which coating achieves GB/T 23445 compliance — it is which type fits your site conditions and hydrostatic exposure. Meeting the standard is the entry requirement; site-fit determines long-term performance.
| Parameter | Type I | Type II | Type III |
|---|---|---|---|
| Elongation at Break | ≥ 200% | ≥ 80% | ≥ 30% |
| Tensile Strength | ≥ 1.2 MPa | ≥ 1.5 MPa | ≥ 1.8 MPa |
| Bond Strength to Concrete | ≥ 0.5 MPa | ≥ 0.6 MPa | ≥ 0.7 MPa |
| Hydrostatic Resistance Waterproofing | Moderate | 0.4 MPa / 30 min | High |
| Typical Application | High-movement substrates | Rooftops, basements, foundations | Rigid structures, sustained pressure |
For most residential and commercial projects, Type II covers the specification requirements without the premium cost of Type III. It has gained wide market acceptance among construction waterproofing buyers in Asia, the Middle East, and Africa.
Parameters confirmed to GB/T 23445 Type II. Full test report for project tender and compliance verification available on request.
| Parameter | Value |
|---|---|
| Type | Two-component JS polymer cement, Type II semi-rigid |
| Mix Ratio | Approx. 1:0.6–0.8 by weight |
| Elongation at Break | ≥ 80% |
| Tensile Strength | ≥ 1.5 MPa |
| Bond Strength to Concrete | ≥ 0.6 MPa |
| Water Tightness | Pass at 0.4 MPa, 30 min |
| Application Rate | 2.0–2.5 kg/m² (2–3 coats) |
| Packaging | 20 kg/set (liquid + powder) |
| MOQ | 1 ton |
| Standard | GB/T 23445 Type II |
| Certifications | CE, ISO 14001 |
Type II is the standard specification for flat rooftop and terrace waterproofing in residential and commercial construction. Moderate elongation, ≥ 0.6 MPa bond strength, and 0.4 MPa water tightness cover rooftop assemblies with light pedestrian traffic or tiled finishes applied over the waterproofing system.
For below-grade structures — basement floors and walls, retaining walls, foundation slabs — Type II's hydrostatic resistance waterproofing and ≥ 0.6 MPa bond strength handle sustained groundwater pressure loads. Compatible with drainage membrane overlays and screed protection layers.
Balcony and podium decks involve thermal cycling and tile finish load demands. Type II elongation handles differential movement at slab edges and service penetrations; brush or roller application adapts to irregular balcony geometry and drainage details.


Shandong Dingtai Waterproof Technology Co., Ltd. is a leading manufacturer based in China' s largest waterproof material production hub-Taitou Industrial Park.As a company with independent import-export rights,we have successfully supplied products across global markets countriesand regions such as North America, Southeast Asia, South America, Africa,Europe and the Middle East. Our commitment to superior quality andreliable service has earned us a strong international reputation andgrowing market presence.

Q1: Why choose us ?
A: We are professional manufacturer, and we can provide the best product ,competitive priceand excellent service.
Q2: Do you provide sample ?ls it free or extra ?
A: Yes,we can provide free sample for quality inspection.According to the regulations of our company , you should assume the freight ,and we will return the freight if you place the order.
Q3: How about the delivery time ?
A: 7-15 days after receive the deposit or LC at sight
Q4: How does your factory do regarding quality control?
A: Quality is priority,. We always attach great importance to quality control from the very beginning to the end. We have a professional QA/QC team to ensure the quality.
Q5: Do you accept OEM or ODM order?
A: Yes, we accept both OEM and ODM for customers.
Q6: What are your terms of delivery?
A: We can accept EXW, FOB, ClF, etc. You can choose one which is the most convenient for you.
Q7: What is the payment way?
A: TT, L/C at sight, West Union,Online Bank Payment.
Q8: Are you trading company or manufacturer?
A: We are manufacturer.So we have a lower price than trading company.
Type II semi-rigid JS polymer cement waterproof coating, 20kg. Balanced polymer-cement ratio for general-purpose waterproofing — rooftops, underground basements, foundations, and civil structures. High bond strength. MOQ 1 ton. CE certified.